RAS Thermal
Datasheet · Type N · Rev. 08

Type N Stranded Wire
Nicrosil / Nisil

Multi-strand twisted Type N wire in 7/19/37 strand builds, for hot and vibrating installs where Type K green-rots.

Multi-strand 7/19/37 — for static runs the solid single strand costs less.

Technical Specifications

Property Specification
Positive Leg Nicrosil (NiCrSi 84.4/14.2/1.4)
Negative Leg Nisil (NiSiMg 95.4/4.4/0.15)
Temperature Range −270°C to +1300°C
Diameter Range φ0.1-5.0 mm
Diameter Tolerance ±0.005mm (fine) / ±0.02mm (standard)
EMF Tolerance ±1.5°C (0-375°C) / ±0.4% (375-1000°C)
Standards IEC 60584-1 Class 1 / ASTM E230 / DIN EN 60584
Surface Finish Bright / Oxidized / Electro-polished
Condition Hard (cold-drawn) / Soft (annealed) / Bright finished
Packaging DIN 125 / 160 / 250 / 355 spool / Coil / Custom reel
Coil Weight 5kg / 10kg / 20kg standard
Minimum Order 10 kg
Lead Time 3-5 business days (stock 0.1-3.0 mm) · 2-3 weeks (non-stock) · 4-6 weeks (custom alloy)
Testing & Traceability 100% eddy-current + resistance + dimensional · MTC · EMF calibration certificate · Furnace batch traceability

How to specify Type N Stranded Wire

  1. Fix the peak temperature and the atmosphere first: a multi-strand N conductor is the default in air.
  2. Take the diameter and the tolerance class from the table above — they set both the response time and the price.
  3. State the temper, the surface finish, the packaging and how deep the certification has to go, then send it to us.

Frequently Asked Questions (FAQ)

What makes Type N more stable than Type K above 1000 °C?

The Nicrosil positive leg (NiCrSi 84.4/14.2/1.4) carries 1.4% silicon, which forms a protective SiO₂ sub-layer and suppresses the chromium oxidation that causes green rot. Drift stays within ±1 °C after 500 h at 1000 °C.

What temperature range and diameters does Type N stranded wire cover?

−270 °C to +1300 °C, in diameters from φ0.1 mm to φ5.0 mm, in 7, 19 or 37 strand constructions.

Why choose stranded Type N rather than solid?

High-temperature or vacuum installations that also vibrate. Heat treatment and turbine work, in short, where a solid conductor would work-harden and break mid-campaign.

You may also need

Bottom line: Type N Stranded Wire to IEC 60584-1 Class 1, with the MTC and EMF calibration certificate per coil.

Add RAS Thermal as a preferred source on Google